LOW RESIDUAL SPRAY PAVING COATING AND METHOD
Application Number |
US2019045441 |
Publication Number |
2020/033503 |
Status |
In Force |
Filing Date |
2019-08-07 |
Publication Date |
2020-02-13 |
Owner |
VENTURE CORPORATION (USA)
|
Inventor |
Spray, Orville
|
Abstract
A paving mixture for application to a surface and a method for the same are provided. The mixture comprises a binding material layer applied to the surface to form a base layer on the surface, and an aggregate material layer applied on top of the binding material layer. The binding material layer can be applied in an amount of at most 0.125 gallons/yd2. The aggregate material layer contains an asphalt mixture that provides a road surface. The aggregate material layer and the binding material layer can be combined on the surface within 30 seconds of application of the binding material layer. Additionally, multiple paving mixtures may be applied to the surface.
IPC Classes ?
- E01C 7/24 - Binder incorporated as an emulsion or solution
- E01C 7/26 - Coherent pavings made in situ made of road-metal and binders of road-metal and bituminous binders mixed with other materials, e.g. cement, rubber, leather, fibre
- E01C 7/18 - Coherent pavings made in situ made of road-metal and binders of road-metal and bituminous binders
|
2.
|
SPRAY PAVING COATING AND METHOD
Application Number |
US2019016615 |
Publication Number |
2019/156960 |
Status |
In Force |
Filing Date |
2019-02-05 |
Publication Date |
2019-08-15 |
Owner |
VENTURE CORPORATION (USA)
|
Inventor |
Spray, Orville
|
Abstract
A paving mixture for application to a surface and a method for the same are provided. The mixture comprises a binding material layer applied to the surface to form a base layer on the surface, and an aggregate material layer applied on top of the binding material layer, wherein the binding material layer comprises at least 13% of the bitumen in the paving mixture by weight, the aggregate material layer contains an asphalt mixture that provides a road surface, and the aggregate material layer and the binding material layer are combined on the surface within 30 seconds of application of the binding material layer.
IPC Classes ?
- E01C 7/35 - Topping or surface dressingsMethods of mixing, impregnating, or spreading them
- E01C 7/18 - Coherent pavings made in situ made of road-metal and binders of road-metal and bituminous binders
- E01C 7/14 - Concrete paving
- E01C 11/00 - Details of pavings
|
3.
|
LOW RESIDUAL SPRAY PAVING COATING AND METHOD
Document Number |
03108420 |
Status |
In Force |
Filing Date |
2019-08-07 |
Grant Date |
2023-09-19 |
Owner |
VENTURE CORPORATION (USA)
|
Inventor |
Spray, Orville
|
Abstract
A paving mixture for application to a surface and a method for the same are provided. The mixture comprises a binding material layer applied to the surface to form a base layer on the surface, and an aggregate material layer applied on top of the binding material layer. The binding material layer can be applied in an amount of at most 0.125 gallons/yd2. The aggregate material layer contains an asphalt mixture that provides a road surface. The aggregate material layer and the binding material layer can be combined on the surface within 30 seconds of application of the binding material layer. Additionally, multiple paving mixtures may be applied to the surface.
IPC Classes ?
- E01C 7/18 - Coherent pavings made in situ made of road-metal and binders of road-metal and bituminous binders
- E01C 7/24 - Binder incorporated as an emulsion or solution
- E01C 7/26 - Coherent pavings made in situ made of road-metal and binders of road-metal and bituminous binders mixed with other materials, e.g. cement, rubber, leather, fibre
|
4.
|
SPRAY PAVING COATING AND METHOD
Document Number |
03089273 |
Status |
In Force |
Filing Date |
2019-02-05 |
Grant Date |
2023-06-27 |
Owner |
VENTURE CORPORATION (USA)
|
Inventor |
Spray, Orville
|
Abstract
A paving mixture for application to a surface and a method for the same are provided. The mixture comprises a binding material layer applied to the surface to form a base layer on the surface, and an aggregate material layer applied on top of the binding material layer, wherein the binding material layer comprises at least 13% of the bitumen in the paving mixture by weight, the aggregate material layer contains an asphalt mixture that provides a road surface, and the aggregate material layer and the binding material layer are combined on the surface within 30 seconds of application of the binding material layer.
IPC Classes ?
- E01C 7/14 - Concrete paving
- E01C 7/18 - Coherent pavings made in situ made of road-metal and binders of road-metal and bituminous binders
- E01C 7/35 - Topping or surface dressingsMethods of mixing, impregnating, or spreading them
- E01C 11/00 - Details of pavings
|
|